Fusible Interlining
|
Techincal
Data Sheet
|
|
Discritpions
|
| |
Basecloth
|
Coating
Method |
| Colour:
|
White
|
Composition:
|
100%Polyester
|
Type: |
Computer
Point |
| Total
Weight: |
60
g/m +
/-10% |
Type: |
Random
Web |
|
|
| Width
|
1
Yard |
Touch:
|
Stiff |
|
|
| Length
|
50
Yard |
|
|
|
|
|
Applications
|
| Various
Garments Reinforcement ( Ladies, Men, Children ) - Jackets - Overcoats
- Shirts - Sleeve Ends - Waist Bands. |
|
Care
Label
|
| |
|
Fusing
Conditions
|
| Smoothing
iron |
Flat
Bed Press |
Continuous
Fusing machine
|
| Temperature: |
150
C |
Temperature: |
150
C |
Temperature: |
135
- 150 C |
| Pressure:
|
Manual |
Pressure:
|
300
g /cm |
Pressure:
|
3
kg |
| Time: |
10/14sec |
Time: |
10/14sec
|
Time: |
10/12sec
|
Frequently
Asked Questions About Our Mattress
|
| |
Points
to be Considered in Choosing Interlining
Interlining
- Must be fit with the thickness of the cloth.
- Must be fit with the type of the cloth.
- Must be fit with the colour of the cloth.
- Should perform against the external effects similarly after fusing
with the cloth.
- Must be suitable for aim of use.
- Must be suitable for the required labelling instruction of the cloth.
- Must be fit with the suggested fusing conditions.
- Must have a cloth-interlining harmony test before production. Customer
should inform the responsible company when necessary.
Performance
Problems in Interlining
- Change of size during the act of fusing
- When fusing temperature is not at the proper value, partial or complete
seperation may be observed both when during time of use and during
cleaning.
- Hardening of parts of the cloth containing the adhesive interlining.
- Diffusion of the adhesive material through the cloth due to inappropriate
fusing conditions.
- The fade of colour in the cloth due to the high temperature and
pressure during fusion.
- Unexpected changes (bubbles, curls) on the surface of the
cloth after washing.
Other weights and touch feel also available :
|
Item
|
Type
|
Specific.
Weight
|
|
Item
|
Type
|
Specific.
Weight
|
|
VHM
120
|
MILD
|
40
g/m2 ± 10%
|
|
VHM
135
|
MILD
|
60
g/m2 ± 10%
|
|
VHS
120
|
STIFF
|
40
g/m2 ± 10%
|
|
VHS
135
|
STIFF
|
60
g/m2 ± 10%
|
|
VHM
125
|
MILD
|
50
g/m2 ± 10%
|
|
VHM
140
|
MILD
|
70
g/m2 ± 10%
|
|
VHS
125
|
STIFF
|
50
g/m2 ± 10%
|
|
VHS
140
|
STIFF
|
70
g/m2 ± 10%
|
|